Forthcoming

Governing role of the secant stiffness at the peak in the low-velocity impact response of curved woven T300/914 panels and the energy-equivalent delamination area

Authors

DOI:

https://doi.org/10.5281/zenodo.23662240

Keywords:

low-velocity impact, woven carbon/epoxy, shell curvature, secant stiffness, cohesive zone model

Abstract

The low-velocity impact response of woven T300/914 carbon/epoxy cylindrical shell panels was solved at six curvature levels extending from the flat plate to the half cylinder, with a constant projected span of 125 mm and a thickness of 1 mm, using SC8R continuum shell models carrying Hashin intralaminar damage and three cohesive interfaces, at an impact energy of 6.70 J. Curvature raises the initial tangent stiffness by 74 per cent while it lowers the peak force by 18 to 23 per cent and extends the contact duration from 17.2 ms to 20.0 to 21.9 ms. This contradiction is resolved by the response being governed by the secant stiffness at the peak in the quasi-static regime, in which the impactor mass is 230 to 370 times the panel mass. The contact duration comes out within 6.4 per cent of the expression π√(m/Ksec) in all six panels, and the peak force stays 3 to 11 per cent below the upper bound √(2E0Ksec). The secant stiffness falls by 25 to 30 per cent from the flat plate to the curved panels, because the flat plate hardens by membrane tension before first damage whereas the curved shell softens by local flattening under the contact. For interlaminar damage, the closed-form relation between the damage variable and the dissipated energy was derived from the bilinear cohesive law, D(d)/Gc = d/(r − (r − 1)d), r = 2GcK/t0², and it was shown that for the card used, with r = 112.6, only 0.9 per cent of the fracture energy is dissipated at the 0.5 level of the damage variable. The energy-equivalent area defined with this relation stays between 122 and 262 mm², while the area of the 0.5 threshold is 3 to 12 times this, the fully separated area is 1.6 to 4.5 times below it, and the fully separated region carries only 22 to 62 per cent of the energy dissipated at the interface. The cohesive area threshold does not represent the delamination energy, and the energy-equivalent area offers a measure independent of the threshold choice. The results belong to a single numerical framework without experimental validation, and the limits of scope are reported.

👁 Abstract Views: 65📥 PDF Downloads: 28

Downloads

Published

2026-10-26

How to Cite

Gök, O., Taşer, H. H., & Gemi, L. (2026). Governing role of the secant stiffness at the peak in the low-velocity impact response of curved woven T300/914 panels and the energy-equivalent delamination area. Journal of Materials and Manufacturing, 5(2), 119–148. https://doi.org/10.5281/zenodo.23662240